X. M. Feng, X. Wang, W. Cai, N. N. Hong, Y. Hu and K. M. Liew (2016) Integrated effect of supramolecular self-assembled sandwich-like melamine cyanurate/MoS2 hybrid sheets on reducing fire hazards of polyamide 6 composites. Journal/Journal Of Hazardous Materials 320 252-264. [In English]
Web link: http://dx.doi.org/10.1016/j.jhazmat.2016.08.012
Keywords: Supramolecular self-assembly; Molybdenum disulfide; Sandwich-like hybrid; sheets; Fire hazards; Catalytic activity; FLAME-RETARDANT POLYAMIDE-6; IN-SITU POLYMERIZATION; HEAT RELEASE; MECHANICAL-PROPERTIES; THERMAL-STABILITY; MOS2; NANOCOMPOSITES; NANOSHEETS; NANOPARTICLES; NANOFILLERS

Abstract: A novel strategy of using supramolecular self-assembly for preparing sandwich-like melamine cyanurate/MoS2 sheets as the hybrid flame retardants for polyamide 6 (PA6) is reported for the first time. The introduction of MoS2 sheets function not only as a template to induce the formation of two-dimensional melamine cyanurate capping layers but also as a synergist to generate integrated flame-retarding effect of hybrid sheets, as well as a high-performance smoke suppressor to reduce fire hazards of PA6 materials. Once incorporating this well-designed structures (4 wt%) into PA6 matrix, there resulted in a remarkable drop (40%) in the peak heat release rate and a 25% reduction in total heat release. Moreover, the smoke production and pyrolysis gaseous products were efficiently suppressed by the addition of sandwich-like hybrid sheets. The integrated functions consisting of inherent flame retarding effect, physical barrier performance and catalytic activity are believed to the crucial guarantee for the reduced fire hazards of PA6 nanocomposites. Furthermore, this novel strategy with facile and scalable features may provide reference for developing various kinds of MoS2 based hybrid sheets for diverse applications. (C) 2016 Elsevier B.V. All rights reserved.

 
 
相关链接
X. M. Feng, X. Wang, W. Cai, N. N. Hong, Y. Hu and K. M. Liew (2016) Journal Of Hazardous Materials 320 252-264.
联系我们
安徽省合肥市金寨路96号
中国科学技术大学
火灾安全全国重点实验室
邮政编码:230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
火灾科学国家重点实验室 版权所有 皖ICP备:002106505 号