首页  科学研究  学术论文  2002年
 
Wang ZZ, Wu GS, Hu Y, Ding Y, Hu KL, Fan WC (2002d) Polymer Degradation and Stability 77(3), 427-434.
文章来源:WOS    作者:SKLFS    发布时间:2011-08-16

Wang ZZ, Wu GS, Hu Y, Ding Y, Hu KL, Fan WC (2002d) Thermal degradation of magnesium hydroxide and red phosphorus flame retarded polyethylene composites. Polymer Degradation and Stability 77(3), 427-434. [In English]

Web link: http://dx.doi.org/10.1016/s0141-3910(02)00099-x

Keywords:

thermal degradation; kinetic analysis; pyrolysis; polyethylene; magnesium hydroxide; red phosphorus; capillary gas-chromatography; copolymers; polymers;

Abstract: The thermal degradation of flame-retarded linear low-density polyethylene (LLDPE) composites containing magnesium hydroxide (MH) and red phosphorus (RP) has been studied by thermogravimetric analysis, real time Fourier transform infrared (FTIR) and pyrolysis gas chromatography mass spectrometry (Py-GC/MS). The Kissinger and Flynn-Wall methods were used to calculate the apparent activation energy (Ea) of the degradation of LLDPE and LLDPE composites. The FTIR studies show that addition of MH to LLDPE improves the thermo-oxidative stability, especially LLDPE/MH composites with suitable amount of RP at higher temperatures. The Py-GC/MS data indicate that incorporation of RP into the LLDPE/MH composite results in a change of pyrolysis mode and thus a great increase of the amounts of compounds with high molecular weights. (C) 2002 Elsevier Science Ltd. All rights reserved.
 
 
相关链接
Wang ZZ, Wu GS, Hu Y, Ding Y, Hu KL, Fan WC (2002d) Polymer Degradation and Stability 77(3), 427-434.
联系我们
安徽省合肥市金寨路96号
中国科学技术大学
火灾安全全国重点实验室
邮政编码:230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
火灾科学国家重点实验室 版权所有 皖ICP备:002106505 号