Zong RW, Hu Y, Liu N, Li S, Liao GX (2007) Investigation of thermal degradation and flammability of polyamide-6 and polyamide-6 nanocomposites. Journal of Applied Polymer Science 104(4), 2297-2303. [In English]

Web link: http://dx.doi.org/10.1002/app.25691

Keywords:

polyamide; nanocomposites; thermogravimetric analysis; activation energy; stability

Abstract: In this paper, polyamide-6 and polyamide-6 nanocomposites were prepared by direct melt intercalation technique. The thermal degradation behavior of both polyamide-6 and polyamide-6 clay nanocomposites has been studied. The apparent activation energy of the nanocomposites is almost the same with that of pure polymer under nitrogen, but the apparent activation energy of the nanocomposites is greatly enhanced in air atmosphere. This increasing trend coincides with the thermal analysis and the cone calorimeter results, which may suggest that the polymer/clay nanocomposites have a higher thermal stability and lower flammability. The kinetic analysis also indicates that the pyrolytic degradation and the thermal oxidative degradation of PA6 and PA6/OMT nanocomposites are two kinds of different reaction models. (c) 2007Wiley Periodicals, Inc.

 
 
相关链接
Zong RW, Hu Y, Liu N, Li S, Liao GX (2007) Journal of Applied Polymer Science 104(4), 2297-2303.
联系我们
安徽省合肥市金寨路96号
中国科学技术大学
火灾安全全国重点实验室
邮政编码:230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
火灾科学国家重点实验室 版权所有 皖ICP备:002106505 号