Wang ZZ, Lv P, Hu Y, Hu KL (2009) Thermal degradation study of intumescent flame retardants by TG and FTIR: Melamine phosphate and its mixture with pentaerythritol. Journal of Analytical and Applied Pyrolysis 86(1), 207-214. [In English]

Web link: http://dx.doi.org/10.1016/j.jaap.2009.06.007

Keywords:

Thermal degradation; Melamine; Melamine phosphate; Pentaerythritol; TG; FTIR; polyphosphate; mechanisms; behavior; systems

Abstract: Thermal degradation of intumescent flame retardants, such as melamine phosphate (MP) and the mixture of MP and pentaerythritol (PER) was studied by TG, FTIR gas analyser (G-FTIR), and FTIR spectrometry. The results indicate that the degradation behavior of MP or PER itself is different from the one of them in the mixture. The volatile degradation products of MP contain mainly NH(3), and H(2)O, as well as small amounts of melamine (MEL), whereas no MEL is found in the degradation of the mixture of MP and PER. Moreover, degradation products of PER are composed of a lot of volatile combustibles such as formaldehydes, alcohols, and C-H compounds except for H(2)O. The mixture of MP and PER, however, produces much less volatile combustibles during its degradation leading to the production of more charring materials. (C) 2009 Elsevier B.V. All rights reserved.

 
 
相关链接
Wang ZZ, Lv P, Hu Y, Hu KL (2009) Journal of Analytical and Applied Pyrolysis 86(1), 207-214.
联系我们
安徽省合肥市金寨路96号
中国科学技术大学
火灾安全全国重点实验室
邮政编码:230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.edu.cn
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
火灾科学国家重点实验室 版权所有 皖ICP备:002106505 号